    Control of InGaAs facets using metal modulation epitaxy (MME)

    Full text link
    Control of faceting during epitaxy is critical for nanoscale devices. This work identifies the origins of gaps and different facets during regrowth of InGaAs adjacent to patterned features. Molecular beam epitaxy (MBE) near SiO2 or SiNx led to gaps, roughness, or polycrystalline growth, but metal modulated epitaxy (MME) produced smooth and gap-free "rising tide" (001) growth filling up to the mask. The resulting self-aligned FETs were dominated by FET channel resistance rather than source-drain access resistance. Higher As fluxes led first to conformal growth, then pronounced {111} facets sloping up away from the mask.Comment: 18 pages, 7 figure

    Origin and implications of the observed rhombohedral phase in nominally tetragonal Pb(Zr\u3csub\u3e0.35\u3c/sub\u3eTi\u3csub\u3e0.65\u3c/sub\u3e)O\u3csub\u3e3\u3c/sub\u3e thin films

    Get PDF
    The structural and electrical properties of Pb(Zr0.35Ti0.65)O3 (PZT) thin films ranging in thickness from 700 to 4000 Å have been investigated. These (001)/(100)-textured films were grown by metalorganic chemical vapor deposition on (111)-textured Ir bottom electrodes. It was observed that, in the as-deposited state, the thinnest PZT films are rhombohedral even though bulk PZT of this composition should be tetragonal. Thicker films have a layered structure with tetragonal PZT at the surface and rhombohedral PZT at the bottom electrode interface. In this article we investigate the origin of this structure and its effect of the ferroelectric and dielectric properties of PZT capacitors. It has been suggested that thin films stresses can affect the phase stability regions of single domain PZT. This possibility has been investigated by piezoresponse microscopy and thin film stress measurements. In the as-deposited state the majority of PZT grains contain a single ferroelastic domain, whereas after a high temperature anneal, a large fraction of the grains contain several ferroelastic domains. Wafer curvature measurements in combination with x-ray diffraction stress measurements in the Ir bottom electrode showed that the as-deposited PZT films are, within experimental error, stress free at room temperature. Landau–Ginbzurg–Devonshire formalism was used to explain the origin of the rhombohedral phase as a result of substrate constraint on single domain PZT grains. Annealing was found to affect the relative volume fractions of the rhombohedral and tetragonal phases and the electrical properties of PZT films. Intermediate temperature anneals increased the volume fraction of the rhombohedral phase and the coercive field extracted from the polarization-electric field hysteresis loops. After a high temperature anneal (650 °C) the majority of the grains transformed into a polydomain state, decreasing the volume fraction of the rhombohedral phase and the coercive field. If the high temperature anneal was performed after deposition of the top electrode, the coercive field became independent of the PZT thickness

    Isolating the photovoltaic junction: atomic layer deposited TiO2-RuO2 alloy Schottky contacts for silicon photoanodes

    Get PDF
    We synthesized nanoscale TiO2-RuO2 alloys by atomic layer deposition (ALD) that possess a high work function and are highly conductive. As such, they function as good Schottky contacts to extract photogenerated holes from n-type silicon while simultaneously interfacing with water oxidation catalysts. The ratio of TiO2 to RuO2 can be precisely controlled by the number of ALD cycles for each precursor. Increasing the composition above 16% Ru sets the electronic conductivity and the metal work function. No significant Ohmic loss for hole transport is measured as film thickness increases from 3 to 45 nm for alloy compositions >= 16% Ru. Silicon photoanodes with a 2 nm SiO2 layer that are coated by these alloy Schottky contacts having compositions in the range of 13-46% Ru exhibit average photovoltages of 525 mV, with a maximum photovoltage of 570 mV achieved. Depositing TiO2-RuO2 alloys on nSi sets a high effective work function for the Schottky junction with the semiconductor substrate, thus generating a large photovoltage that is isolated from the properties of an overlying oxygen evolution catalyst or protection layer

    Origin and passivation of fixed charge in atomic layer deposited aluminum oxide gate insulators on chemically treated InGaAs substrates

    Get PDF
    We report experimental and theoretical studies of defects producing fixed charge within Al(2)O(3) layers grown by atomic layer deposition (ALD) on In(0.53)Ga(0.47)As(001) substrates and the effects of hydrogen passivation of these defects. Capacitance-voltage measurements of Pt/ALD-Al(2)O(3)/n-In(0.53)Ga(0.47)As suggested the presence of positive bulk fixed charge and negative interfacial fixed charge within ALD-Al(2)O(3). We identified oxygen and aluminum dangling bonds (DBs) as the origin of the fixed charge. First-principles calculations predicted possible passivation of both O and Al DBs, which would neutralize fixed charge, and this prediction was confirmed experimentally; postmetallization forming gas anneal removed most of the fixed charge in ALD-Al(2)O(3). (C) 2010 American Institute of Physics. (doi:10.1063/1.3399776
    • …